Home
>
PRODUCTS
>
Steel Pipe Steel Tube
>
Scaffold tube is treated badly: it gets dropped, bent, walked on and left out in the rain for a year, then it has to carry a working platform. EN39 and BS1139 exist because generic galvanized pipe does not survive that duty. This 48.3 mm tube with a 3.2 mm wall is made specifically to those standards, with the wall tolerance held on the heavy side because a scaffold tube that thins to 3.0 mm loses about 12 percent of its bending capacity, and the tube is hot dipped after forming to a zinc coating of at least 60 micrometres local.
The tests that matter are the ones buyers rarely ask for until there is an accident: tensile, yield, elongation, flattening without cracking, and a bending or load test on the finished tube. We test each lot for tensile and flattening, and we can supply the load test report to EN39 Annex A on request. Ends are cut square and deburred, because a burred end tears gloves and damages the coupler thread on the next tube in the stack.
Key Features| Parameter | Specification |
|---|---|
| Product | Hot dipped galvanized scaffolding steel pipe |
| Standard | EN39, BS1139 Part 1, EN 10240 |
| Outside diameter | 48.3 mm |
| Wall thickness | 3.2 mm (3.0 mm and 4.0 mm available) |
| Length | 6 m standard, 1 m to 6.5 m cut lengths |
| Tensile strength | 360 - 510 MPa |
| Yield strength | 235 MPa minimum |
| Elongation | 15 percent minimum |
| Zinc coating | 60 micrometre minimum local, 505 g/m2 typical |
| Straightness | 1.5 mm per metre maximum |
| Test | Tensile, flattening, load test on request |
| Ends | Square cut and deburred |
This tube is used for tube and coupler scaffolding systems, birdcage scaffolds, formwork support, falsework towers, mobile tower scaffolds and temporary edge protection. It is also used for event staging frames and racking where a certified scaffold tube is required by the client.
If the tubes will be powder coated or painted over the zinc, tell the coating shop that the surface is galvanized and needs a suitable primer, or the paint will flake within a season. For rental fleets, we recommend 3.2 mm wall rather than 3.0 mm, because the heavier wall survives repeated inspection cycles and reduces the reject rate at the yard.
Inspection, Documentation and PackagingLot testing covers tensile strength, yield, elongation and flattening, with wall thickness gauged at both ends and at mid length, plus straightness and zinc coating mass checks. Load testing to EN39 Annex A can be performed and reported per lot, and each bundle carries a test certificate reference that matches the packing list.
Tubes are bundled in 61 piece bundles, strapped with galvanized banding and capped at both ends to keep water out during storage. Bundle weight stays within forklift and crane limits, and bundles are marked with standard, size, heat number and test certificate number for site records.
Buyer Questions We Answer Before OrderingCan you supply 3.0 mm wall for a lighter rental fleet? Yes, 3.0 mm is available, but for rental use we recommend 3.2 mm because the reject rate after repeated inspection is significantly lower.
Do you provide EN39 load test reports? Yes, load and bending tests to EN39 Annex A can be performed and reported per lot, referenced on the bundle tag.
Is the tube galvanized inside? Yes, it is dipped as a whole so the bore is coated, which is what prevents internal rust bleeding out of the ends.
Contact Us at Any Time