Steel Pipe Steel Tube
>
Chrome moly pipe is specified for one reason: carbon steel loses creep strength above about 425 degrees C and P11 or P22 does not. P11 carries 1.25 percent chromium with 0.5 percent molybdenum and holds useful strength to roughly 540 degrees C, while P22 with 2.25 percent chromium and 1 percent molybdenum extends that to about 590 degrees C. This pipe is supplied at 168.3 mm outside diameter, Sch80, 12 m length, normalized and tempered, and certified to ASTM A335.
The metallurgy matters as much as the chemistry. A335 requires the pipe to be heat treated, and the tempering temperature has to be high enough that the hardness stays within the range that will not crack during field welding and post weld heat treatment. We record hardness on each lot and can supply a hardness survey along the length for buyers who will weld without a subsequent PWHT, which is common on small bore instrument and drain lines.
Key Features| Parameter | Specification |
|---|---|
| Product | Chrome moly alloy steel seamless pipe |
| Standard | ASTM A335 / ASME SA335 |
| Grades | P11, P22, P5, P9, P91 on request |
| Outside diameter | 168.3 mm (6 inch) |
| Wall thickness | 10.97 mm (Sch80) |
| Length | 12 m, SRL and DRL available |
| Chemistry P11 | Cr 1.00 - 1.50, Mo 0.44 - 0.65 |
| Chemistry P22 | Cr 1.90 - 2.60, Mo 0.87 - 1.13 |
| Tensile strength | 415 MPa minimum |
| Yield strength | 205 MPa minimum |
| Heat treatment | Normalized and tempered |
| Test | Hydrostatic, ultrasonic on request |
Use cases are main steam and hot reheat piping, boiler outlet headers, high temperature process lines in refineries and petrochemical plants, and hydrogen or synthesis gas lines where the alloy content resists hydrogen attack at elevated temperature and pressure.
Two engineering notes worth raising early. First, P22 has limited resistance to thermal fatigue at weld joints, so support design and expansion loops matter as much as the pipe grade. Second, field welding requires preheat in the 200 to 300 degrees C range and a post weld heat treatment, and the PWHT temperature must stay below the mill tempering temperature; we supply the mill tempering record so the welding procedure can be set correctly.
Inspection, Documentation and PackagingTesting covers chemistry per heat, tensile and yield per lot, hardness survey, hydrostatic test and dimensional inspection at both ends. Ultrasonic inspection of the pipe body is available for higher consequence service, and a positive material identification report can be issued for each bundle so the alloy grade is confirmed at receipt.
Bundles are strapped and separated with dunnage, ends are capped, and each length is stenciled with heat number, grade and size. Because chrome moly pipe is often held in plant stores for years, we apply a rust preventive that can be removed with solvent before welding rather than a heavy varnish that has to be ground off.
Buyer Questions We Answer Before OrderingCan you supply P91 as well as P11 and P22? Yes, P5, P9 and P91 are produced on the same line, with P91 supplied quenched and tempered and hardness capped per A335.
Do you provide the tempering temperature record? Yes, the certificate states the austenitizing and tempering temperatures for each heat, which the welding procedure needs for PWHT limits.
Is positive material identification included? PMI can be added per bundle using X-ray fluorescence, with a report listing the chromium and molybdenum readings.